Fig. (3) Compressive strength of fly ash based geopolymer mortars versus curing time with incorporation of: (a) 10% Calcium hydroxide; (b) 10%Portland cement; and (c) 5%Portland cement; (d) 10%Metakaolin; and (e) 20%Metakaolin.