Table 7: Mix Proportions (kg/m3)

Sample Cement Fine Aggregate Coarse Aggregate Water Superplasticizer Sisal Fiber
M0.0 380 730 1400 203.67 1.9 0.0
M0.5 380 730 1400 203.67 1.9 1.9
M1.0 380 730 1400 203.67 1.9 3.8
M1.5 380 730 1400 203.67 1.9 5.7
M2.0 380 730 1400 203.67 1.9 7.6