Table 1: Mix properties of geopolymer concrete.

Groups Iron Filings
%
Metakaolin kg/m3 Sand kg/m3 Gravel
kg/m3
Alkaline Solution Lit/m3 Water Lit/m3 Sp
%
A,B 0
0.5
0.75
1.0
400 720 1100 180 40 3