Table 5: Average roughness Ra and standard deviation measured for procedure C (samples finished with diamond milling cutters and successively polished).

Procedure Ra [μm] Std dev [μm]
ESTHET X HD C1 1.556 0.130
CERAM-X MONO C1 1.444 0.096
FILTEK SILORANE C1 0.469 0.249
ESTHET X HD C2I 1.023 0.091
CERAM-X MONO C2I 0.764 0.139
FILTEK SILORANE C2I 0.257 0.029
ESTHET X HD C2II 1.318 0.198
CERAM-X MONO C2II 0.712 0.085
FILTEK SILORANE C2II 0.535 0.166
ESTHET X HD C2III 1.311 0.084
CERAM-X MONO C2III 1.218 0.176
FILTEK SILORANE C2III 0.853 0.585