Table 6: Average roughness Ra and standard deviation measured for procedure D (samples finished with tungsten carbide multi-blade milling cutters and successively polished).
|
Procedure |
Ra [μm] |
Std dev [μm] |
ESTHET X HD |
D1 |
0.868 |
0.071 |
CERAM-X MONO |
D1 |
0.751 |
0.105 |
FILTEK SILORANE |
D1 |
0.319 |
0.008 |
|
|
|
|
ESTHET X HD |
D2I |
0.252 |
0.108 |
CERAM-X MONO |
D2I |
0.212 |
0.085 |
FILTEK SILORANE |
D2I |
1.022 |
0.644 |
|
|
|
|
ESTHET X HD |
D2II |
0.485 |
0.103 |
CERAM-X MONO |
D2II |
0.721 |
1.103 |
FILTEK SILORANE |
D2II |
0.257 |
0.060 |
|
|
|
|
ESTHET X HD |
D2III |
0.475 |
0.151 |
CERAM-X MONO |
D2III |
0.455 |
0.109 |
FILTEK SILORANE |
D2III |
0.342 |
0.021 |