Table 4: Fracture toughness of the carburized layer under different ratios of σscsb.

σscsb σsc /MPa KICc/MPa·m1/2
1.0 855 5.03
1.25 1068 6.29
1.5 1282 7.55
2.0 1710 10.06
2.5 2137 12.58